Trade-Off Between Water-Absorption Reduction and Strength-Gap Recovery at Three KH560 Treatment-Solution Concentrations for Airport-Pavement Recycled-Aggregate Concrete

Lihao Liu, Lei Xi, Mengming Li, Gaoyun Song

Open source

DOI
10.3390/ma19184006
Published
2026-09-20
Container
Materials
Publisher
MDPI AG
Open access
unknown

Credibility signals

uncertain Score 64/100 under policy 1.0.0. This is a metadata assessment, not a judgment of the paper's conclusions.

Show all credibility signals

Cite this work

BibTeX

@article{allodium:10.3390/ma19184006,
  title = {Trade-Off Between Water-Absorption Reduction and Strength-Gap Recovery at Three KH560 Treatment-Solution Concentrations for Airport-Pavement Recycled-Aggregate Concrete},
  author = {Lihao Liu and Lei Xi and Mengming Li and Gaoyun Song},
  year = {2026},
  journal = {Materials},
  doi = {10.3390/ma19184006},
  url = {https://doi.org/10.3390/ma19184006}
}

RIS

TY  - JOUR
TI  - Trade-Off Between Water-Absorption Reduction and Strength-Gap Recovery at Three KH560 Treatment-Solution Concentrations for Airport-Pavement Recycled-Aggregate Concrete
AU  - Lihao Liu
AU  - Lei Xi
AU  - Mengming Li
AU  - Gaoyun Song
PY  - 2026
JO  - Materials
DO  - 10.3390/ma19184006
UR  - https://doi.org/10.3390/ma19184006
ER  - 

APA

Liu, L., Xi, L., Li, M., & Song, G. (2026). Trade-Off Between Water-Absorption Reduction and Strength-Gap Recovery at Three KH560 Treatment-Solution Concentrations for Airport-Pavement Recycled-Aggregate Concrete. Materials. https://doi.org/10.3390/ma19184006

Source records